Hardness Conversion Chart: Rockwell, Brinell, and Vickers

Written by Azmi Anees on November 17, 2026

A hardness conversion chart helps engineers compare Rockwell, Brinell, and Vickers readings when working with different metal specifications. Each method measures a material's resistance to indentation, but uses a different indenter, test force, and measurement process. 

Knowing how these scales relate makes it easier to review material certificates, check heat-treated components, and confirm whether a metal meets its specified hardness requirements.


How Do Rockwell, Brinell, and Vickers Hardness Tests Work?

Before comparing hardness values, it helps to understand how each testing method works. The main difference is how the indenter creates an impression in the material and how the resulting measurement is calculated.

Rockwell Hardness (HR)

The Rockwell test measures the depth of an indentation under an applied load. A testing machine applies an initial force, followed by a larger force, and measures the permanent change in indentation depth.

Two commonly used scales are:

  • Rockwell C (HRC): Uses a diamond cone indenter and is commonly used for hardened steels and other hard materials.
  • Rockwell B (HRB): Uses a ball indenter and is suitable for softer metals, including annealed steels and copper alloys.

Rockwell testing is popular in production environments because it provides quick readings without requiring an operator to measure the indentation under a microscope.

Brinell Hardness (HBW)

The Brinell test presses a tungsten carbide ball into the material under a specified force. The diameter of the resulting indentation is measured to calculate the hardness value. It is commonly used for castings, forgings, and larger metal components. The larger indentation helps assess hardness over a wider area, making it useful for materials with less uniform structures.

Vickers Hardness (HV)

The Vickers test uses a diamond pyramid indenter pressed into the material under a controlled force. The two diagonals of the resulting indentation are measured to calculate hardness. Vickers testing works across a broad hardness range by using different test forces. It is particularly useful for thin sections, small components, surface treatments, and checking hardness changes across a material's cross-section.

Read more: What Is Thermal Shock Resistance?


Rockwell, Brinell, and Vickers Hardness Conversion Table

The following table provides approximate equivalent values for non-austenitic steels, including carbon, alloy, and tool steels. It is based on ASTM E140, Table 1.

Rockwell C (HRC)Brinell (HBW)Vickers (HV)
20226238
25253266
30286302
35327345
40371392
45421446
50481513
55560595
60(654)697
65(739)832

Note: Values in parentheses indicate approximate Brinell equivalents outside the range normally used for Brinell testing. A dash indicates that no applicable equivalent is provided. These conversions apply to non-austenitic steels and may not be suitable for other metals or alloys.


How to Choose the Right Hardness Testing Method

The right testing method depends on the material, component size, surface condition, and inspection requirements.

Consider the following factors:

  • Material hardness: Rockwell C is commonly used for hardened steels, while Rockwell B suits softer metals. Vickers covers a wider range of hardness levels.
  • Component size: Brinell is useful for larger components and castings. Vickers can measure smaller areas and thin sections.
  • Surface condition: Roughness, scale, coatings, and surface damage can affect indentation readings. Proper surface preparation is important.
  • Testing requirements: Always check the engineering drawing, material specification, or customer requirements before selecting a test.

For example, a large steel casting may be better suited to Brinell testing, while a thin hardened layer may require Vickers testing to assess its hardness without measuring too much of the underlying material.

Check out: Ductile-to-Brittle Transition Temperature


Why Hardness Conversion Values Are Not Always Exact

Although conversion tables make comparisons easier, different hardness tests do not measure the same material response. Several factors can affect the relationship between readings.

  • Material composition: Different alloys can produce different indentation responses, even when their measured hardness values appear similar.
  • Heat treatment: Annealing, quenching, and tempering change a metal's microstructure and hardness. These changes can affect the relationship between different scales.
  • Surface condition: Oxidation, decarburization, roughness, and coatings can influence test results.
  • Test conditions: Indenter geometry, applied force, specimen thickness, and surface preparation all affect measurements.

ASTM E140 and ISO 18265 provide standardized conversion relationships for specified material groups. These standards also explain the limitations of using converted values. When a drawing or customer specification requires a particular hardness scale, direct testing using that method is the preferred approach. A converted result should not automatically be treated as proof of compliance.


Where Hardness Conversion Is Used in Heat Treatment

Hardness conversions help engineers compare test results across different stages of manufacturing and heat treatment. They are useful when reviewing material certificates, inspecting finished components, or comparing supplier reports. 

However, converted values should not replace direct testing when a specific hardness scale is required. Teams should use calibrated equipment, follow applicable standards, and record original test results alongside converted values.

You might like to know the Welding Heat Input Formula


Need Support With Industrial Heat Treatment?

AxiomHT provides industrial heat treatment expertise and technical support to help manufacturers achieve consistent processing results.

Contact our team to discuss your application and requirements.


Frequently Asked Questions (FAQs)

It helps engineers compare approximate hardness values across different testing scales, including Rockwell, Brinell, and Vickers.

HRC uses a diamond cone indenter for harder materials, while HRB uses a ball indenter for softer metals.

Yes, standardized conversion tables provide approximate equivalents when the material falls within the applicable conversion range.

Rockwell C is commonly used for hardened steel, while Vickers suits thin sections and localized hardness measurements.

No, conversion values are approximate and depend on material composition, microstructure, heat treatment, and testing conditions.

ASTM E140 and ISO 18265 provide standardized guidance and conversion tables for comparing hardness values across different scales.

Related Posts

On-Site Heat Treatment Specialists. Providing Electrical resistance, Combustion, Induction, and more.
Axiom Heat Treatment BBB Business Review
California714-655-3205
Axiom Heat Treatment
2755 N Gaviota Ave, Signal Hill, CA 90755, United States
© 2026 Axiom HT All Rights Reserved | Call: 714-655-3205 | Powered By Ouroai LLC